FORD FLTM BI 112-02
TUKON HARDNESS OF PAINT
active, Most Current
Buy Now
| Organization: | FORD |
| Publication Date: | 19 March 2001 |
| Status: | active |
| Page Count: | 2 |
scope:
Application
This method is used to determine the microhardness of paint and is performed by indenting the paint film with a standard Knoop indenter by application of a 25 g load.