NEN-EN-ISO 11409

Plastics - Phenolic resins - Determination of heats and temperatures of reaction by differential scanning calorimetry

active, Most Current
Organization: NEN
Publication Date: 1 September 1998
Status: active
Page Count: 18
ICS Code (Thermosetting materials): 83.080.10
scope:

The principle of the method specified is measuring the heat flux supplied to a test sample as a function of time or temperature, while the test sample is subjected to a temperature schedule under a specified atmosphere. A reaction is marked by the release of energy from the sample, resulting in an exothermic peak in the heating curve. Integration of the recorded peak area as a function of time gives a measure of the energy of the reaction. Applies to phenolic resins with exothermic behaviour, such as resols or mixtures of novolaks with hexamethylenetetramine or other curing agents.

Document History

NEN-EN-ISO 11409
September 1, 1998
Plastics - Phenolic resins - Determination of heats and temperatures of reaction by differential scanning calorimetry
The principle of the method specified is measuring the heat flux supplied to a test sample as a function of time or temperature, while the test sample is subjected to a temperature schedule under a...