TAPPI - T 569 OM
Internal Bond Strength (Scott Type)
inactive
| Organization: | TAPPI |
| Publication Date: | 1 January 2007 |
| Status: | inactive |
| Page Count: | 7 |
Document History
January 1, 2022
Internal bond strength (Scott type)
This method defines a test that measures the energy required to rapidly delaminate a sheet-type specimen. The “Z” directional rupture is initiated by the impact of a pendulum having both a controlled...
January 1, 2014
Internal bond strength (Scott type)
This method defines a test that measures the energy required to rapidly delaminate a sheet-type specimen. The "Z" directional rupture is initiated by the impact of a pendulum having both a controlled...
January 1, 2009
Internal bond strength (Scott type)
This method defines a test that measures the energy required to rapidly delaminate a sheet-type specimen. The "Z" directional rupture is initiated by the impact of a pendulum having both a controlled...
T 569 OM
January 1, 2007
Internal Bond Strength (Scott Type)
A description is not available for this item.
January 1, 2000
Internal Bond Strength (Scott Type)
A description is not available for this item.