API RP 5L3
Recommended Practice for Conducting Drop-Weight Tear Tests on Line Pipe
inactive
Buy Now
| Organization: | API |
| Publication Date: | 1 March 1969 |
| Status: | inactive |
| Page Count: | 8 |
scope:
These procedures describe a recommended method for conducting drop-weight tear tests on line pipe, 20 in. OD and larger, with wall thicknesses 0.750 in. and less.
Document History
August 1, 2014
Drop-Weight Tear Tests on Line Pipe
These procedures describe a recommended method for conducting Drop-Weight Tear Tests to measure the fracture appearance or fracture ductility of the pipe as referenced in API 5L.
August 1, 2014
Drop-Weight Tear Tests on Line Pipe
These procedures describe a recommended method for conducting Drop-Weight Tear Tests to measure the fracture appearance or fracture ductility of the pipe as referenced in API Specification 5L,...
August 1, 2014
Drop-Weight Tear Tests on Line Pipe
These procedures describe a recommended method for conducting Drop-Weight Tear Tests to measure the fracture appearance or fracture ductility of the pipe as referenced in API Specification 5L,...
August 1, 2014
Drop-Weight Tear Tests on Line Pipe
These procedures describe a recommended method for conducting Drop-Weight Tear Tests to measure the fracture appearance or fracture ductility of the pipe as referenced in API Specification 5L,...
February 1, 1996
Recommended Practice for Conducting Drop-Weight Tear Tests on Line Pipe
These procedures describe a recommended method for conducting drop-weight tear tests to measure the fracture appearance or fracture ductility of line pipe as referenced in API Specification 5L,...
February 1, 1996
Recommended Practice for Conducting Drop-Weight Tear Tests on Line Pipe
These procedures describe a recommended method for conducting drop-weight tear tests to measure the fracture appearance or fracture ductility of line pipe as referenced in API Specification 5L,...
March 1, 1978
RECOMMENDED PRACTICE FOR CONDUCTING DROP-WEIGHT TEAR TESTS ON LINE PIPE SECOND EDITION
A description is not available for this item.
March 1, 1978
RECOMMENDED PRACTICE FOR CONDUCTING DROP-WEIGHT TEAR TESTS ON LINE PIPE
These procedures describe a recommended method for conducting drop-weight tear tests on line pipe, 20 in. OD and larger, with wall thicknesses 1.562 in. and less.
API RP 5L3
March 1, 1969
Recommended Practice for Conducting Drop-Weight Tear Tests on Line Pipe
These procedures describe a recommended method for conducting drop-weight tear tests on line pipe, 20 in. OD and larger, with wall thicknesses 0.750 in. and less.