FORD WSS-M4D840-A5
ACETAL (POM) COPOLYMER, MOLDED-IN-COLOR, INTERIOR, LOW GLOSS, MELT FLOW RATE 11 – 18 g/10 MINUTES ***TO BE USED WITH FORD WSS-M99P1111-A***
active, Most Current
Buy Now
| Organization: | FORD |
| Publication Date: | 13 July 2011 |
| Status: | active |
| Page Count: | 7 |
scope:
The material defined by this specification is a molded-in-color, low gloss thermoplastic acetal copolymer based on trioxane for interior use.
Document History
FORD WSS-M4D840-A5
July 13, 2011
ACETAL (POM) COPOLYMER, MOLDED-IN-COLOR, INTERIOR, LOW GLOSS, MELT FLOW RATE 11 – 18 g/10 MINUTES ***TO BE USED WITH FORD WSS-M99P1111-A***
The material defined by this specification is a molded-in-color, low gloss thermoplastic acetal copolymer based on trioxane for interior use.
May 8, 2007
ACETAL (POM) COPOLYMER, MOLD IN COLOR MOLDING COMPOUND, INTERIOR, LOW GLOSS - ***TO BE USED WITH FORD WSS-M99P1111-A***
The material defined by this specification is a thermoplastic acetal copolymer based on trioxane.