NR/GN/TRK/9023 ISSUE 1

Tri Metallic Zone Weld Repair

active, Most Current
Organization: NR
Publication Date: 5 March 2022
Status: active
Page Count: 15
scope:

This procedure applies to weld repairs to tri-metallic zones.

The requirements for weld repairs to Tri Metallic Zones can be found in NR/L2/TRK/0132 Mod02 Clause 6, Repairs to Tri-Metallic Welds (TMZ) on AMS crossing leg end extensions.

NOTE: Weld repairs to tri-metallic zones (TMZ's) are not permitted within 300mm of the stainless-steel insert on the 260-grade rail or 20mm on the AMS grade rail.

Purpose 

To provide a repair procedure within tri-metallic zones to improve asset life, availability, and cost saving.

Document History

NR/GN/TRK/9023 ISSUE 1
March 5, 2022
Tri Metallic Zone Weld Repair
This procedure applies to weld repairs to tri-metallic zones. The requirements for weld repairs to Tri Metallic Zones can be found in NR/L2/TRK/0132 Mod02 Clause 6, Repairs to Tri-Metallic Welds...