SAE International - AMS5843D
Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged
active
Buy Now
| Organization: | SAE International |
| Publication Date: | 1 October 2000 |
| Status: | active |
description:
This specification covers a high strength, corrosion and heat resistant cobalt-nickel-chromi
Document History
AMS5843D
October 1, 2000
Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged
This specification covers a high strength, corrosion and heat resistant cobalt-nickel-chromium alloy in the form of bars.