FORD - WSK-M4D895-A2
POLYBUTYLENE TEREPHTHALATE + ACRYLONITRILE STYRENE ACRYLATE BLEND (PBT+ASA), 20% GLASS FIBER REINFORCED MOLDING COMPOUND, INTERIOR ***TO BE USED WITH FORD WSS-M99P1111-A***
inactive
| Organization: | FORD |
| Publication Date: | 27 June 2006 |
| Status: | inactive |
| Page Count: | 6 |
scope:
The materials defined by these specifications are 20% glass fiber reinforced blends of polybutylene terephthalate and acrylonitrile-styren
Document History
January 20, 2010
POLYBUTYLENE TEREPHTHALATE + ACRYLONITRILE STYRENE ACRYLATE BLEND (PBT+ASA), 20% GLASS FIBER REINFORCED MOLDING COMPOUND, INTERIOR ***TO BE USED WITH FORD WSS-M99P1111-A***
The materials defined by these specifications are 20% glass fiber reinforced blends of polybutylene terephthalate and acrylonitrile-styrene-acrylate (PBT+ASA). WSK-M4D895-A2 and WSK-M4D895-A3...
WSK-M4D895-A2
June 27, 2006
POLYBUTYLENE TEREPHTHALATE + ACRYLONITRILE STYRENE ACRYLATE BLEND (PBT+ASA), 20% GLASS FIBER REINFORCED MOLDING COMPOUND, INTERIOR ***TO BE USED WITH FORD WSS-M99P1111-A***
The materials defined by these specifications are 20% glass fiber reinforced blends of polybutylene terephthalate and acrylonitrile-styrene-acrylate (PBT+ASA). WSK-M4D895-A2 and WSK-M4D895-A3...
April 3, 1995
POLYBUTYLENE TEREPHTHALATE + ACRYLONITRILE STYRENE ACRYLATE BLEND (PBT+ASA), 20 %
1. SCOPE The materials defined by these specifications are 20 % glass fiber reinforced blends of polybutylene terephthalate and acrylonitrile-styrene-acrylate (PBT+ ASA). WSK-M4D895-A2 and...