DIN - WL 2.4682 Beiblatt 1
High temperature cobalt cast alloy with about 0.5C-26Cr-11Ni-7.5W; investment casting
inactive, Most Current
| Organization: | DIN |
| Publication Date: | 1 January 1977 |
| Status: | inactive |
| Page Count: | 2 |
| ICS Code (DINGCD26): | DINGCD26 |
| ICS Code (Other materials): | 49.025.99 |
Document History
January 1, 1977
Hochwarmfeste Kobalt-Guss-Legierung mit etwa 0,5C-26Cr-11Ni-7,5W; Feinguss
A description is not available for this item.
WL 2.4682 Beiblatt 1
January 1, 1977
High temperature cobalt cast alloy with about 0.5C-26Cr-11Ni-7.5W; investment casting
A description is not available for this item.