scope:
I Scope The test serves to evaluate the corrosion protection of organic andlor inorganic coatings (e.g. oil, wax, paint, plastic or metallic subcoatings) on metals under the influence of accelerated outdoor exposure. The check simulates the infiltration initiated by a defined damage of the coating, surface corrosion and blistering.
Document History
November 23, 2015
Accelerated Outdoor Exposure
The test serves to evaluate the corrosion protection of organic and/or inorganic coatings (e.g. oil, wax, paint, plastic or metallic subcoatings) on metals under the influence of accelerated outdoor...
GME 60411
April 1, 1997
Accelerated Outdoor Exposure
I Scope The test serves to evaluate the corrosion protection of organic andlor inorganic coatings (e.g. oil, wax, paint, plastic or metallic subcoatings) on metals under the influence of accelerated...