FORD WSB-M4D840-A4
ACETAL (POM) COPOLYMER, COLOR PIGMENTED MOLDING COMPOUND, MELT FLOW RATE 1.8 - 4.0, INTERIOR ***TO BE USED WITH FORD WSS-M99P1111-A***
inactive
Buy Now
| Organization: | FORD |
| Publication Date: | 29 September 2006 |
| Status: | inactive |
| Page Count: | 5 |
scope:
The material defined by this specification is a thermoplastic acetal copolymer based on trioxane.
Document History
February 23, 2021
ACETAL (POM) COPOLYMER, COLOR PIGMENTED MOLDING COMPOUND, MELT FLOW RATE 1.8 - 4.0, INTERIOR ***TO BE USED WITH FORD WSS-M99P1111-A***
The material defined by this specification is a thermoplastic acetal copolymer based on trioxane.
FORD WSB-M4D840-A4
September 29, 2006
ACETAL (POM) COPOLYMER, COLOR PIGMENTED MOLDING COMPOUND, MELT FLOW RATE 1.8 - 4.0, INTERIOR ***TO BE USED WITH FORD WSS-M99P1111-A***
The material defined by this specification is a thermoplastic acetal copolymer based on trioxane.
June 12, 1995
ACETAL (POM) COPOLYMER, MELT FLOW RATE 1.8 - 4.0, INTERIOR
1. SCOPE The material defined by this specification is a thermoplastic acetal copolymer based on trioxane.