DIN EN 4826
Aerospace series - Zinc-nickel (12 % to 16 % Ni) plating of steels with specified tensile strength ≤ 1450 MPa, copper alloys and aluminium alloys for parts and fasteners; German and English version FprEN 4826:2014
inactive
| Organization: | DIN |
| Publication Date: | 1 August 2014 |
| Status: | inactive |
| Page Count: | 32 |
| ICS Code (Coatings and related processes used in aerospace industry): | 49.040 |
Document History
March 1, 2015
Aerospace series - Zinc-Nickel (12 % to 16 % Ni) plating of steels with specified tensile strength ≤ 1 450 MPa, copper alloys, nickel alloys and aluminium alloys for parts and fasteners; German and English version EN 4826:2014
Diese Norm legt die Beschichtung einer Zink-Nickel-Legierung (12 % bis 16 %) an mechanischen Verbindungsteilen und Verschlüssen aus Stahl (Rm ≤ 1 450 MPa), nichtrostenden Stählen (Rm ≤ 1 450 MPa),...
DIN EN 4826
August 1, 2014
Aerospace series - Zinc-nickel (12 % to 16 % Ni) plating of steels with specified tensile strength ≤ 1450 MPa, copper alloys and aluminium alloys for parts and fasteners; German and English version FprEN 4826:2014
A description is not available for this item.