NAVISTAR CEMS GT-19
VOID - Early Water Resistance Of Sealers And Paints
inactive, Most Current
Buy Now
| Organization: | NAVISTAR |
| Publication Date: | 1 August 2015 |
| Status: | inactive |
| Page Count: | 1 |
Document History
NAVISTAR CEMS GT-19
August 1, 2015
VOID - Early Water Resistance Of Sealers And Paints
A description is not available for this item.
August 1, 2009
Early Water Resistance Of Sealers And Paints
This is a method for evaluating the ability of the paint film to withstand water induced degradation in the incomplete stage of drying.
August 1, 2001
Early Water Resistance of Sealers and Paints
1.0 SCOPE This is a method for evaluating the ability of the paint film to withstand water induced degradation in the incomplete stage of drying.
July 1, 1999
Early Water Resistance of Sealers and Paints
1.0 SCOPE This is a method for evaluating the ability of the paint film to withstand water induced degradation in the incomplete stage of drying.