This specification covers two platinum-iridium alloys in the form of rod, wire, strip, and sheet material for electrical contacts. Raw materials shall be of such quality and purity that the finished product (produced by cold working, annealing, turning, grinding, or pickling as required) will have...
This specification covers the standard requirements for wrought zirconium and zirconium alloy seamless and welded tubes for nuclear applications except for nuclear fuel cladding. Five grades of reactor grade zirconium and zirconium alloys with R60001, R60802, R60804, R60901, and R60904 UNS number...
This specification covers virgin poly(L-lactic acid) resin (PLLA resin) intended for use in surgical implants. This specification does not cover stereoisomeric compositions based on various D, L, or DL copolymer ratios. This specification addresses material characteristics of virgin poly(L-lactic...
This standard defines the requirements for fully replacing undesirable surface finishes using robotic hot solder dip. Requirements for qualifying and testing the refinished piece parts are also included. This standard covers the replacement of pure tin and Pb-free tin alloy finishes...
1.1 This test method describes the analysis of titanium and its alloys by spark atomic emission spectrometry (Spark-AES) and glow discharge atomic emission spectrometry (GD-AES). The titanium specimen to be analyzed may be in the form of a disk, casting, foil, sheet, plate, extrusion, or some other...
1.1 This method describes the analysis of titanium and titanium alloys, such as specified by committee B10, by inductively coupled plasma atomic emission spectrometry (ICP-AES) and direct current plasma atomic emission spectrometry (DCP-AES) for the following elements: Element Application Range (wt...
This specification covers aluminum-base and zinc-base master alloys used to make zinc die-casting alloys. The material may be made by any suitable process. The material covered by this specification shall be of uniform quality and shall be free of dross, flux, or other harmful contamination. If the...
This specification covers refined iridium as sponge and powder in two grades, Grade 99.80 (UNS PO6100) and Grade 99.90. The metal may be produced by any refining process. They shall conform to the required chemical composition for iridium, rhodium, platinum, palladium, ruthenium, lead, silicon,...
This specification covers tinned hard-drawn and medium-hard-drawn round copper wire for electrical properties. The tinned wire shall be made by coating hard-drawn and medium-hard-drawn copper wire with commercially pure tin. The copper shall be of such quality and purity that...
This specification covers refined cadmium metal in slab, ball or stick form. The cadmium shall be furnished in commercial standard forms or shapes. The cadmium supplied shall conform to the chemical requirements for one of the three grades, L01951, L01971, L01981. The producer may obtain...
This specification covers refined palladium as sponge, cast bar, and wrought forms in one grade designated as Grade 99.95 (UNS PO3995). The metal may be produced by any refining process that yields a product capable of meeting the chemical composition requirements prescribed for palladium, platinum...
This specification covers five grades of zirconium strip, sheet, and plate. These are low oxygen zirconium (Grade R60700), unalloyed zirconium (Grade R60702), zirconium-tin (Grade R60704), zirconium-niobium (Grade R60705), and zirconium-niobium (Grade R60706). The materials shall be made...
This specification covers two commercial zinc alloys, namely: Slush Casting Alloy A (Z34510) and Slush Casting Alloy B (Z30500), in ingot form for remelting for the manufacture of castings. This slush casting alloys are used primarily for the manufacture of hollow castings such as lighting...
1.1 This specification2 covers 39 grades of annealed titanium and titanium alloy forgings as follows: 1.1.1 Grade F-1-UNS R50250. Unalloyed titanium, 1.1.2 Grade F-2-UNS R50400. Unalloyed titanium, 1.1.2.1 Grade F-2H-UNS R50400. Unalloyed titanium (Grade 2 with 58 ksi (400 MPa) minimum UTS), 1.1.3...
1.1 This specification2 covers annealed titanium and titanium alloy bars and billets as follows: 1.1.1 Grade 1-UNS R50250. Unalloyed titanium, 1.1.2 Grade 2-UNS R50400. Unalloyed titanium, 1.1.2.1 Grade 2H-UNS R50400. Unalloyed titanium (Grade 2 with 58 ksi [400 MPa] minimum UTS), 1.1.3 Grade 3-UNS...
1.1 This specification covers cored, annular, concentric-lay-stran
1.1 This test method covers the determination of silver in the range of 13 µg/g to 500 µg/g by acid dissolution of the silver and measurement by atomic absorption spectrometry. Copper concentrates are internationally traded within the following content ranges: Element Unit Content Range Aluminum %...
This specification covers the standard general requirements for lead-coated and lead-alloy-coated, round, soft or annealed copper wire for electrical purposes. The base metal shall be made of copper while the coating material shall be a commercially pure lead or a lead alloy which consists of lead,...
This practice details the recommended method for calculating the equivalent boron content (EBC) values of nuclear elements and materials that are of potential significance as thermal neutron poisons. EBC factors are determined from the atomic weight of elements and the thermal neutron absorption...