DIN 50969-3

Prevention of hydrogen-induced brittle fracture of high-strength steel building elements - Part 3: Post operational influences and extended testing

inactive
Buy Now
Organization: DIN
Publication Date: 1 August 2017
Status: inactive
Page Count: 18
ICS Code (Iron and steel products in general): 77.140.01

Document History

June 1, 2018
Vermeidung fertigungsbedingter wasserstoffinduzierter Sproedbrueche bei hochfesten Bauteilen aus Stahl - Teil 3: Nachtraeglich betriebsbedingte Einfluesse und erweiterte Pruefungen
Dieser Teil von DIN 50969 legt Verfahren zur Beurteilung des Wasserstoffgefährdungspotentials und zum Nachweis einer vorliegenden Sprödbruchgefährdung bei der Korrosionsbelastung von Bauteilen aus...
DIN 50969-3
August 1, 2017
Prevention of hydrogen-induced brittle fracture of high-strength steel building elements - Part 3: Post operational influences and extended testing