DS/EN 60811-512

Electric and optical fibre cables - Test methods for non-metallic materials - Part 512: Mechanical tests - Methods specific to polyethylene and polypropylene compounds - Tensile strength and elongation at break after conditioning at elevated temperature

active, Most Current
Buy Now
Organization: DS
Publication Date: 3 August 2012
Status: active
Page Count: 14
ICS Code (Cables): 29.060.20
scope:

IEC 60811-512:2012 describes the procedure for testing tensile strength and elongation at break after conditioning at elevated temperature. It is specific to polyethylene and polypropylene compounds. This test is intended for samples from filled cables, of polyolefin insulations with a wall thickness of more than 0,8 mm and for polyolefin sheaths in direct contact with filling compound. IEC 60811-512:2012 cancels and replaces Clause 8 of IEC 60811-4-2:2004, which is withdrawn. Full details of the replacements are shown in Annex A of IEC 60811-100:2012. There are no specific technical changes with respect to the previous edition, but see the Foreword to IEC 60811-100:2012.[
]
This publication is to be read in conjunction with IEC 60811-100:2012.

Document History

DS/EN 60811-512
August 3, 2012
Electric and optical fibre cables - Test methods for non-metallic materials - Part 512: Mechanical tests - Methods specific to polyethylene and polypropylene compounds - Tensile strength and elongation at break after conditioning at elevated temperature
IEC 60811-512:2012 describes the procedure for testing tensile strength and elongation at break after conditioning at elevated temperature. It is specific to polyethylene and polypropylene compounds....
Electric and optical fibre cables - Test methods for non-metallic materials -- Part 512: Mechanical tests - Tensile strength and elongation at break after conditioning at elevated temperature - Methods specific to polyethylene and polypropylene compounds
This Part 512 of IEC 60811 describes the procedure for testing tensile strength and elongation at break after conditioning at elevated temperature. It is specific to polyethylene and polypropylene...