TAPPI - T205 SP
Forming handsheets for physical tests of pulp
| Organization: | TAPPI |
| Publication Date: | 1 January 2012 |
| Status: | inactive |
| Page Count: | 10 |
scope:
This procedure describes a method of forming test handsheets at an oven dry weight of 60 g/m2 for determining the physical properties of pulp for both unrefined and refined pulps. Appendix B describes a modified procedure for making heavier weight sheets for pulps intended for use in paperboard manufacture.
The procedures for measuring the physical properties are described in TAPPI T 220 "Physical Testing of Pulp Handsheets."
The procedure for forming handsheets for determining the optical properties of pulp is described in TAPPI T 218 "Forming Handsheets for Reflectance Tests of Pulp."
A method for measuring the drainage time and drainage factor of pulp is described in TAPPI T 221 "Drainage Time of Pulp."