GMNA - 9984808
Primer (Adhesion Promoter) - Waterborne for TPO
inactive
Buy Now
| Organization: | GMNA |
| Publication Date: | 1 September 1998 |
| Status: | inactive |
| Page Count: | 2 |
scope:
1 SCOPE. This specification covers the requirements for waterborne adhesion promoters for thermoplastic olefins (TPO). This adhesion promoter may be conductive or nonconductive depending on the needs of the user.
Document History
November 1, 2021
High Bake Adhesion Promoter - Waterborne for TPO
This specification covers the requirements for a high bake 121 °C (250 °F) waterborne (WB) adhesion promoter for Thermoplastic Polyolefin (TPO). The adhesion promoter may be conductive or...
April 1, 2019
High Bake Adhesion Promoter - Waterborne for TPO
This specification covers the requirements for a high bake 121 °C (250 °F) waterborne (WB) adhesion promoter for Thermoplastic Polyolefin (TPO). The adhesion promoter may be conductive or...
July 1, 2015
High Bake Adhesion Promoter - Waterborne for TPO
This specification covers the requirements for a high bake 121 °C (250 °F) waterborne adhesion promoter for Thermoplastic Polyolefin (TPO). The adhesion promoter may be conductive or nonconductive...
9984808
September 1, 1998
Primer (Adhesion Promoter) - Waterborne for TPO
1 SCOPE. This specification covers the requirements for waterborne adhesion promoters for thermoplastic olefins (TPO). This adhesion promoter may be conductive or nonconductive depending on the needs...
January 1, 1995
Primer (Adhesion Promoter) - Waterborne or Baked Solventborne
A description is not available for this item.