FORD - WSK-M4D643-A2
POLYPROPYLENE (PP), HOMOPOLYMER, 40% MINERAL FILLED, MELT FLOW RATE 1 - 3.5
inactive
| Organization: | FORD |
| Publication Date: | 3 November 2000 |
| Status: | inactive |
| Page Count: | 7 |
scope:
1. SCOPE
The materials defined by these specifications are 40 % mineral filled injection molding compounds based on polypropylene homopolymer.
Document History
March 23, 2011
POLYPROPYLENE (PP), HOMOPOLYMER 40% MINERAL FILLED, MELT FLOW RATE 1 - 3.5 ***TO BE USED WITH FORD WSS-M99P1111-A***
The materials defined by these specifications are 40% mineral filled injection molding compounds based on polypropylene homopolymer.
October 11, 2005
POLYPROPYLENE (PP), HOMOPOLYMER 40% MINERAL FILLED, MELT FLOW RATE 1 - 3.5 ***TO BE USED WITH FORD WSS-M99P1111-A***
The materials defined by these specifications are 40% mineral filled injection molding compounds based on polypropylene homopolymer.
WSK-M4D643-A2
November 3, 2000
POLYPROPYLENE (PP), HOMOPOLYMER, 40% MINERAL FILLED, MELT FLOW RATE 1 - 3.5
1. SCOPE The materials defined by these specifications are 40 % mineral filled injection molding compounds based on polypropylene homopolymer.
July 3, 1989
POLYPROPYLENE (PP), HOMOPOLYMER, 40% MINERAL FILLED, MELT FLOW RATE 1 - 3.5