scope:
1.1 This test method covers the measurement of tensile strength (breaking strength) and stretch properties (elongation and "F" value) for pressure-sensitive tapes. It includes procedures for machine- direction and cross-direction tests and tests for tapes with low and high stretch and reinforced backings. It also includes a procedure for obtaining stretch force ("F" value) in conjunction with a determination of tensile strength. These procedures employ a constant-rate-of-ext
1.2 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Note 1-A complete metric companion to Test Method D3759 has been developed-D3759M; therefore, no metric equivalents are presented in this test method. Test Method D3759M uses specimen widths of 12 mm and 24 mm rather than 1/2 in. and 1 in. used in Test Method D3759. This difference in test parameters will generally produce lower values for Test Method D3759M.