STYRENE MALEIC ANHYDRIDE COPOLYMER (SMA), RUBBER MODIFIED, 16 % GLASS FIBER
inactive
| Organization: | FORD |
| Publication Date: | 10 November 1994 |
| Status: | inactive |
| Page Count: | 7 |
Document History
May 16, 2006
STYRENE MALEIC ANHYDRIDE COPOLYMER (SMA), RUBBER MODIFIED, 16 % GLASS FIBER REINFORCED MOLDING COMPOUND ***TO BE USED WITH FORD WSS-M99P1111-A***
The material defined by this specification is a rubber modified, 16% glass fiber reinforced, styrene maleic anhydride copolymer thermoplastic molding compound. The glass fibers are coated with a...
April 27, 2001
STYRENE MALEIC ANHYDRIDE COPOLYMER (SMA), RUBBER MODIFIED, 16 % GLASS FIBER REINFORCED MOLDING COMPOUND
1. SCOPE The material defined by this specification is a rubber modified, 16 % glass fiber reinforced, styrene maleic anhydride copolymer thermoplastic molding compound. The glass fibers are coated...
May 18, 2000
STYRENE MALEIC ANHYDRIDE COPOLYMER (SMA), RUBBER MODIFIED, 16 % GLASS FIBER REINFORCED MOLDING COMPOUND
1. SCOPE The material defined by this specification is a rubber modified, 16 % glass fiber reinforced, styrene maleic anhydride copolymer thermoplastic molding compound. The glass fibers are coated...
December 17, 1997
STYRENE MALEIC ANHYDRIDE COPOLYMER (SMA), RUBBER MODIFIED, 16 % GLASS FIBER REINFORCED MOLDING COMPOUND
1. SCOPE The material defined by this specification is a rubber modified, 16 % glass fiber reinforced, styrene maleic anhydride copolymer thermoplastic molding compound. The glass fibers are coated...
WSB-M4D857-A2
November 10, 1994
STYRENE MALEIC ANHYDRIDE COPOLYMER (SMA), RUBBER MODIFIED, 16 % GLASS FIBER
A description is not available for this item.